Glass filber need felt
1 Finishing treatment: PTFE dip forming process
Glass filber need felt
1) Weight:800g/m2
2) Thickness:2.4mm
3) Tensile strength (n/5x10cm) warp:1,505 weft:1,800
4) Tensile elongation(%): warp: 10 weft:15
5) Air permeability (L/m2 x S):35-60
6) Working temperature:270°C-290°C
7) Finishing treatment: PTFE dip forming process